BEIYE GH625 Wrought Superalloy top 10

Overview of GH625 Wrought Superalloy

 

GH625 high temperature alloy is a nickel-base alloy having excellent stress-rupture properties and good oxidation resistance to 1200F. It is recommended for jet engine components, aerospace applications and chemical processing equipment. As a benchmark material among modern wrought superalloys, it remains consistently accessible through global super alloy precision suppliers specializing in high-temperature solutions.

 

The Typical Applications of This Alloy are

Jet engine components

 

Aerospace equipment

 

Chemical processing construction

 

Sea-water equipment

 

* Typical values for material tested in accordance with GB/T 4340.3, GB/T 228, GB/T 22315.

 

Heat Treatment

Annealing: Mill annealing is accomplished by heating at 930~1040℃ for up to one hour.

 

Solution Annealing: Heat to 1100~1200℃ and cool in air or quench.

 

Stress Relieving: Heat at 900℃ for times commensurate with thickness and cool.

 

If you want to know more about our nickel-based superalloys and their technical specifications, please do not hesitate to contact Beiye, your reliable partner for precision alloy and supply.

 

If you want to know more about n06625 alloy and alloy 625 uns, please visit our website.

 

Enjoyed this article? Stay informed by joining our newsletter!

Comments

You must be logged in to post a comment.

About Author

Founded in 1960 named Beijing Metallurgical Research Institute, the largest metallic functional materials R&D manufacturing base in China, renamed Beijing Beiye Functional Materials Corporation (for short: Beiye) in July, 2005 and also turned from a state owned enterprise into a privately owned company. As a national high-tech enterprise, we concentrate on supplying qualified precision alloy, superalloys, and special stainless steels for the power electronic industry, the aerospace industry, the electric locomotive industry and the automobile industry. At the same time, we have been keeping very close cooperation relation with many famous universities and research institutes. https://www.beiye-alloy.com/

Recent Articles
Nov 24, 2026, 1:56 AM Pizza Depot
Nov 24, 2026, 1:26 AM KQBD Trang xem kết quả bóng đá trực tuyến nhanh và chính xác nhất
Nov 24, 2026, 1:23 AM Pizza Depot