BEIYE GH536 Wrought Superalloy top 10

Overview of GH536 Wrought Superalloy

 

GH536 is a nickel-chromium-iron-molybdenum hastelloy x alloy that possesses an exceptional combination of oxidation resistance, fabricability and high-temperature strength. This high-temperature alloy has been found to be exceptionally resistant to stress-corrosion cracking in petrochemical applications.Below 900℃, it has moderate stress rupture and creep strength, cold and hot working formability and good weldability. GH536 alloy is widely used in gas-turbine engines, industrial furnace applications, and chemical process industries. Similar wrought alloy's names in different standards:

 

Beiye

China

America

France

Germany

Britain

GH536

GH3536

HastelloyX

NC22FeD

NiCr22FeMo

Nimonic PE13

 

The Typical Applications of This Alloy are

Honeycomb seal structure

 

Fuel conduit

 

Combustor components

 

* 0.6mm thick strip sample

 

Heat Treatment

In-process annealing: To relieve all strains and restore the alloy to a soft condition suitable for further cold rolling or drawing, forming, bending or similar operations, anneal at 1065~1150℃ for not more than 1 hour. Since the high nickel, high permeability alloys readily absorb carbon, sulfur, oxygen and other contaminants from combustion furnace gasses, in-process annealing should be conducted in hydrogen, vacuum or inert gas atmospheres.

 

Final annealing: For maximum softness and optimum magnetic electrical properties, the cold deformed GH536 alloy should be solution treated in an oxygen-free, dry hydrogen atmosphere at 1065~1150℃ with air cooling, and the heat treatment time is determined based on the strip thickness.

 

In order to ensure the quality of the strip surface, oil, grease, lacquer and all other contaminants must be removed before annealing.

 

For professional guidance on heat treatment processes and reliable material sourcing, please contact Beiye, your trusted partner in precision alloy and supply.

 

As a precision alloy manufacturing company, we can provide kinds of precision alloy for sale, anything you need, please contact us.

 

Enjoyed this article? Stay informed by joining our newsletter!

Comments

You must be logged in to post a comment.

About Author

Founded in 1960 named Beijing Metallurgical Research Institute, the largest metallic functional materials R&D manufacturing base in China, renamed Beijing Beiye Functional Materials Corporation (for short: Beiye) in July, 2005 and also turned from a state owned enterprise into a privately owned company. As a national high-tech enterprise, we concentrate on supplying qualified precision alloy, superalloys, and special stainless steels for the power electronic industry, the aerospace industry, the electric locomotive industry and the automobile industry. At the same time, we have been keeping very close cooperation relation with many famous universities and research institutes. https://www.beiye-alloy.com/

Recent Articles
Nov 24, 2026, 1:56 AM Pizza Depot
Nov 24, 2026, 1:26 AM KQBD Trang xem kết quả bóng đá trực tuyến nhanh và chính xác nhất
Nov 24, 2026, 1:23 AM Pizza Depot